Page: 1 / 9 Total 85 questions

Want more questions? Get Premium Access.

Question 1

[Installation Procedures]

Newly applied cast linings must cure before stripping the forms per the:

Correct Answer: A. manufacturer's recommendations.

Question 2

[Inspection and Testing Requirements]

What is the size of a test specimen for permanent linear change of refractories?

Correct Answer: D. 2 in. (50 mm) x 2 in. (50 mm) x 9 in. (230 mm)

Question 3

[Inspection and Testing Requirements]

As-installed gunned test specimens are prepared by cutting specimens with a:

Correct Answer: A. diamond saw

Question 4

[Responsibilities and Qualifications]

Conflicts in documents and/or drawings shall be resolved by the:

Correct Answer: B. owner.

Question 5

[Installation Procedures]

The lining surface should remain uncovered and free from contact with moisture during the curing period for what type of refractory?

Correct Answer: A. Chemically bonded

Question 6

[Material Requirements]

When is metal fiber reinforcement used in castable refractory?

Correct Answer: D. Only when specified by the owner

Question 7

[Terms, Definitions, and Abbreviations]

Refractory abrasion is defined as the wearing away of the surface by:

Correct Answer: B. the scouring action of moving solids.

Question 8

[Acceptance Criteria]

Which of the following is a valid acceptance criterion for cold crushing strength of castable used in erosive service?

Correct Answer: C. All individual values must exceed 75% of the manufacturer's minimum published CCS.

Question 9

[Responsibilities and Qualifications]

Which of the following is the inspector responsible for?

Correct Answer: A. Hammer testing newly installed linings

Question 10

[Material Requirements]

The term "shelf life" refers to the maximum time:

Correct Answer: A. material may be stored and remains in usable condition.